Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 122 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 - 122 °C
196 - 252 °F
Average value: 105 °C Grade Count:84
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Copyright © lookpolymers.com All Rights Reserved