Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 105 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 - 105 °C
212 - 221 °F
ASTM D1525, HDT Method B
Loxim 500 00V0 Polycarbonate/Acrylonitrile Butadiene Styrene
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 100 - 105 °C
212 - 221 °F
ASTM D1525, HDT Method B
Loxim 810 02T HB Polypropylene Compound, 10% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 85.0 - 105 °C
185 - 221 °F
Average value: 95.4 °C Grade Count:7
Overview of materials for Acrylic, UV Stabilized, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of..