Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 230 °C @Time <=180000 sec |
446 °F @Time <=50.0 hour |
IEC 60216/T1 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Maximum Service Temperature, Air | 230 °C @Time <=180000 sec |
446 °F @Time <=50.0 hour |
IEC 60216/T1 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |