Polymer Property : Maximum Service Temperature, Air = 284 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 140 °C

@Time <=86400 sec
284 °F

@Time <=24.0 hour
Murtfeldt Murytal® C Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..
Maximum Service Temperature, Air 140 °C

@Time <=86400 sec
284 °F

@Time <=24.0 hour
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..
Maximum Service Temperature, Air 140 °C

@Time <=86400 sec
284 °F

@Time <=24.0 hour
Murtfeldt Murytal® ESD Acetal Copolymer, Conductive
Additives make this material conductive. The mechanical properties of the material are retained almost in their entirety. Special Properties:• High rigidity• Excellent ability to regain its form•..
Maximum Service Temperature, Air 140 °C

@Time 7.20e+7 sec
284 °F

@Time 20000 hour
IEC 60216/T1
Raschig Group AMPLA® 2500 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat..