Maximum Service Temperature, Air 85.0 °C

@Time 1.80e+7 sec
185 °F

@Time 5000 hour
Murtfeldt Murylon® B Nylon 6
Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope..