Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 115 °C @Time 1.80e+7 sec |
239 °F @Time 5000 hour |
|
Murtfeldt Murytal® C Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Maximum Service Temperature, Air | 115 °C @Time 1.80e+7 sec |
239 °F @Time 5000 hour |
|
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |
|||
Maximum Service Temperature, Air | 115 °C @Time 1.80e+7 sec |
239 °F @Time 5000 hour |
|
Murtfeldt Murylat® SP Polyethylene Terephthalate Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri.. |