Polymer Property : Maximum Service Temperature, Air = 1020 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 550 °C

@Time 1.80e+7 sec
1020 °F

@Time 5000 hour
Inhomogeneous Heating
Schott Nextrema® 724-5 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Maximum Service Temperature, Air >= 550 °C

@Time 1.80e+7 sec
>= 1020 °F

@Time 5000 hour
Homogeneous Heating
Schott Nextrema® 724-5 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Maximum Service Temperature, Air 550 °C

@Time 1.80e+7 sec
1020 °F

@Time 5000 hour
Inhomogeneous Heating
Schott Nextrema® 724-8 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..