Polymer Property : CTE, linear = 95.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 172 µm/m-°C

@Temperature 100 - 150 °C
95.6 µin/in-°F

@Temperature 212 - 302 °F
UV Postcure; ASTM E831-05
DSM Somos® GP Plus 14122
Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually ..