Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.6 µm/m-°C @Temperature 100 °C |
9.79 µin/in-°F @Temperature 212 °F |
|
AK Steel 13-4 SR® Ferritic Stainless Steel AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w.. |