Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.52 µm/m-°C @Temperature 0.000 - 300 °C |
5.29 µin/in-°F @Temperature 32.0 - 572 °F |
|
Corning 0159 Lead Barium Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated. |
|||
CTE, linear | 9.52 µm/m-°C @Temperature 0.000 - 300 °C |
5.29 µin/in-°F @Temperature 32.0 - 572 °F |
|
Corning 0159 Lead Barium Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated. |