Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.04 µm/m-°C @Temperature 20.0 - 100 °C |
9.467 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel 334 (UNS S33400) Allegheny Ludlum Type 334 is a titanium- and aluminum-bearing austenitic stainless steel offering superior elevated temperature scaling resistance compared to the conventional chromium-nickel stainl.. |