Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.30 - 9.30 µm/m-°C @Temperature 20.0 - 400 °C |
4.61 - 5.17 µin/in-°F @Temperature 68.0 - 752 °F |
|
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy Inflection point 460°C. A nickel-iron controlled-expansion alloy containing 48% nickel. Its coefficient of thermal expansion is designed to match that of soft lead and soda-lime glasses. The a.. |