Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 156 µm/m-°C @Temperature 50.0 - 100 °C |
86.7 µin/in-°F @Temperature 122 - 212 °F |
ASTM E831-00 |
DSM Somos® 14120 Water-resistant resin for stereolithography, White DescriptionDSM Somos® 14120 is a low viscosity liquid photopolymer that produces strong, tough, water-resistant parts. Parts created with Somos® 14120 have a white, opaque appearance similar to p.. |
|||
CTE, linear | 156 µm/m-°C @Temperature -60.0 - 50.0 °C |
86.7 µin/in-°F @Temperature -76.0 - 122 °F |
DIN 53122 |
Arkema Group ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved Information provided by Arkema Group |