Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 86.0 µm/m-°C @Temperature <=31.0 °C |
47.8 µin/in-°F @Temperature <=87.8 °F |
below Tg |
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Clear is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to .. |
|||
CTE, linear | 86.0 µm/m-°C @Temperature -40.0 °C |
47.8 µin/in-°F @Temperature -40.0 °F |
|
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
CTE, linear | 86.0 µm/m-°C @Temperature 5.00 - 20.0 °C |
47.8 µin/in-°F @Temperature 41.0 - 68.0 °F |
Below Tg |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |
|||
CTE, linear | 86.0 µm/m-°C @Temperature <=31.0 °C |
47.8 µin/in-°F @Temperature <=87.8 °F |
below Tg |
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m.. |