Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 147 - 155.4 µm/m-°C @Temperature 100 - 150 °C |
81.7 - 86.33 µin/in-°F @Temperature 212 - 302 °F |
ASTM E831-00 |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
CTE, linear | 147 µm/m-°C @Temperature 20.0 °C |
81.7 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 2; Perkin Elmer TMS-2 |
Aptek 6500-PMF Electrically conductive epoxy adhesive High purity, low outgassing, electrically conductive adhesiveAPTEK 6500-PMF is a one component, pre-mixed frozen, 100% solid, silver-filled epoxy adhesive specifically designed for microelectronic d.. |
|||
CTE, linear | 147 µm/m-°C @Temperature 20.0 °C |
81.7 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 2 |
Aptek DAT-A-THERM 1000 Electrically insulating urethane film DAT-A-THERM 1000 is a tough, flexible, void free, electrically insulating urethane film designed to fill air gaps and dissipate heat between devices and substrates. DAT-A-THERM 1000 film is a 100% s.. |