Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 146 µm/m-°C @Temperature 100 - 200 °C |
81.0 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
3M Dyneon™ CC622 PTFE 10% Graphite Filled
(discontinued **) Product Form: Black, pelletized free-flowing powder. Applications include bearings, ring seals.Data provided by Dyneon. |
|||
CTE, linear | 146 µm/m-°C @Temperature 100 - 200 °C |
81.0 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
3M Dyneon™ TR 1105 PTFE
(discontinued **) Ideal for thin wall ram extrusion productsReduces cold flow and melt viscosityLower permeabilityLower porosityWeldableExcellent product smoothnessIncreased machine outputInformation provided by Dyne.. |