Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 75.0 - 80.0 µm/m-°C @Temperature 25.0 - 100 °C |
41.7 - 44.4 µin/in-°F @Temperature 77.0 - 212 °F |
ASTM D696 |
Polikim EFALON® K-35 PTFE, 35% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |