Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.6 µm/m-°C @Temperature 427 - 649 °C |
8.10 µin/in-°F @Temperature 800 - 1200 °F |
|
Crucible Steel PEERLESS A Tool Steel, AISI H21 Peerless A is designed for tools which will run hot, at operating temperatures between about 600F and 1100F. The tools should not be water cooled in service, due to a high risk of thermal shock. Pee.. |
|||
CTE, linear | 14.6 µm/m-°C @Temperature 20.0 - 399 °C |
8.10 µin/in-°F @Temperature 68.0 - 750 °F |
|
Carlson 904L Austenitic Stainless Steel General Description904L is an austenitic nickel-chromium stainless steel with molybdenum and copper additions. The elevated nickel and chromium content of 904L make it resistant to corrosion in a w.. |