Polymer Property : CTE, linear = 750 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 750 µm/m-°C

@Temperature -17.8 - 0.000 °C
417 µin/in-°F

@Temperature 0.000 - 32.0 °F
ChevronTexaco Texatherm®
Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging ..