Polymer Property : CTE, linear = 70.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 127 µm/m-°C

@Temperature -60.0 - 50.0 °C
70.6 µin/in-°F

@Temperature -76.0 - 122 °F
DIN 53122
Arkema Group ORGASOL® 3502 D Nat 1 Copolyamide 6/12
Information provided by Arkema Group