Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.36 µm/m-°C @Temperature 21.0 - 538 °C |
7.978 µin/in-°F @Temperature 69.8 - 1000 °F |
|
Latrobe LSS™ L6 Tool Steel (ASTM L6) TLS L6 tool steel is a versatile, oil-hardening tool steel that is characterized by very good toughness. TLS L6 tool steel is suitable for use as tools, dies, and machine parts which require a good .. |