Polymer Property : CTE, linear = 7.90 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 14.2 µm/m-°C

@Temperature 20.0 - 199 °C
7.90 µin/in-°F

@Temperature 68.0 - 390 °F
Carlson 2205 (UNS S31803) Duplex Stainless Steel
General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist..
CTE, linear 14.2 µm/m-°C

@Temperature 20.0 - 199 °C
7.90 µin/in-°F

@Temperature 68.0 - 390 °F
Carlson 2205 (UNS S32205) Duplex Stainless Steel
General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist..
CTE, linear 14.2 µm/m-°C

@Temperature 21.1 - 316 °C
7.90 µin/in-°F

@Temperature 70.0 - 600 °F
Carlson C 600 Nickel-Chromium-Iron Alloy
Carlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excellent resistance to c..
CTE, linear 14.2 µm/m-°C

@Temperature 21.1 - 316 °C
7.90 µin/in-°F

@Temperature 70.0 - 600 °F
Carlson C 600ESR Nickel-Chromium-Iron Alloy
General DescriptionCarlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excell..