Polymer Property : CTE, linear = 7.70 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 13.9 µm/m-°C

@Temperature 20.0 - 538 °C
7.70 µin/in-°F

@Temperature 68.0 - 1000 °F
Crucible Steel CSM® 6 Tool Steel, AISI A6
CSM 6 is an air hardening tool steel offering moderate wear resistance and toughness. It may be hardened from a low hardening temperature for easy heat treatment.Information provided by Crucible Ind..
CTE, linear 13.9 µm/m-°C

@Temperature 3.33 - 399 °C
7.70 µin/in-°F

@Temperature 38.0 - 750 °F
hardness of 40 HRC
Bohler-Uddeholm UDDEHOLM ALVAR 14 Hot Work Tool Steel
Alvar 14 is a chromium-nickel-molybdenumvanadium alloyed steel ALVAR 14 is characterized by: Good toughnessGood resistance to high thermal stresses Good stability in hardeningGood through-hardening..