Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.77 µm/m-°C @Temperature 21.0 - 316 °C |
7.650 µin/in-°F @Temperature 69.8 - 601 °F |
Mean; Annealed and Aged |
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Heat capacity, melting range, moduli, and Poisson's ratio re.. |
|||
CTE, linear | 13.77 µm/m-°C @Temperature 21.0 - 316 °C |
7.650 µin/in-°F @Temperature 69.8 - 601 °F |
Mean |
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed + Aged Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Typical aging - 1750°F (954°C)/1 h/AC plus 1325°F (.. |