Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.33 µm/m-°C @Temperature 25.0 - 400 °C |
7.406 µin/in-°F @Temperature 77.0 - 752 °F |
|
Carpenter S7 Alloy Tool Steel (AISI S7) Carpenter S7 is a general purpose air hardening tool steel having high impact and shock resistance. It has good resistance to softening at moderately high temperatures. This combination of propertie.. |