Polymer Property : CTE, linear = 7.244 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 13.04 µm/m-°C

@Temperature 100 °C
7.244 µin/in-°F

@Temperature 212 °F
Special Metals INCONEL® alloy 693
INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t..