Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.0 µm/m-°C @Temperature 93.3 °C |
7.24 µin/in-°F @Temperature 200 °F |
|
Special Metals UDIMET® alloy L-605 Co-Cr-W-Ni Alloy UDIMET® alloy L-605 (UNS R30605) is a solid solution strengthened cobalt-chromium-tungsten-nickel alloy with excellent high-temperature strength and excellent oxidation resistance to 2000°F (1093°.. |