Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.9 µm/m-°C @Temperature 20.0 - 499 °C |
7.16 µin/in-°F @Temperature 68.0 - 930 °F |
|
Bohler-Uddeholm BÖHLER K340 ISODUR® Premium Cold Work Steel BÖHLER K340 ISODUR is a universal cold work tool steel with which you‘ll be making money and just when blanking coins, but also when: blanking, cutting, cold rolling, extruding, deep drawing and b.. |