Polymer Property : CTE, linear = 7.02 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 7.02 µm/m-°C

@Temperature -73.3 - 21.1 °C
3.90 µin/in-°F

@Temperature -100 - 70.0 °F
Crucible Steel 154 CM Martensitic Steel
Crucible 154 CM is a modification of 440C martensitic stainless steel to which molybdenum has been added. 154 CM has better corrosion resistance, better wear resistance and better hot-hardness than ..
CTE, linear 7.02 µm/m-°C

@Temperature -74.0 - 21.0 °C
3.90 µin/in-°F

@Temperature -101 - 69.8 °F
Crucible Steel CPM® 154 Tool Steel
CPM 154 is CPM-manufactured version of Crucible’s standard 154 CM. The CPM manufacturing process produces a uniform distribution of the carbides in this grade, giving this CPM 154 easier grinding a..
CTE, linear 7.02 µm/m-°C

@Temperature 316 °C
3.90 µin/in-°F

@Temperature 600 °F
ATI Wah Chang Nb/Nb Alloy C-103
This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig..
CTE, linear 7.02 µm/m-°C

@Temperature 260 °C
3.90 µin/in-°F

@Temperature 500 °F
ATI Wah Chang Zircadyne® Alloy Zr 702
Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A..