Thermal Properties Metric English Comments
CTE, linear 118.4 µm/m-°C

@Temperature 60.0 - 110 °C
65.78 µin/in-°F

@Temperature 140 - 230 °F
Y direction
CRP Technology Windform® LX 2.0 Polyamide Composite
Processed by selective laser sintering (SLS). Windform® LX 2.0 has improved the already excellent performances of Windform® LX and this can be noticed from technical properties and sinterability ..