Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 63.5 µm/m-°C @Temperature 100 - 200 °C |
35.3 µin/in-°F @Temperature 212 - 392 °F |
ASTM E-233 |
UBE UPIMOL® R Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |