Polymer Property : CTE, linear = 61.28 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 101.2 - 110.3 µm/m-°C

@Temperature 0.000 - 50.0 °C
56.22 - 61.28 µin/in-°F

@Temperature 32.0 - 122 °F
ASTM E831-00
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons..