Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.48 µm/m-°C @Temperature 20.0 - 600 °C |
6.933 µin/in-°F @Temperature 68.0 - 1110 °F |
|
Latrobe CSS-42L™ VIM-VAR High Performance Carburizing Stainless Steel; Bearing and Gear Steel CSS-42L™ is a case carburizable stainless steel alloy intended to be used at operating temperatures up to 800°F (427°C). The alloy is able to achieve and maintain a high surface hardness .. |
|||
CTE, linear | 12.48 µm/m-°C @Temperature 25.0 - 250 °C |
6.933 µin/in-°F @Temperature 77.0 - 482 °F |
|
Carpenter O6 Graphitic Tool Steel (AISI O6) Carpenter O6 is an oil-hardening tool steel designed for cold work applications. It is designed to have free graphite in the microstructure. This free graphite is responsible for the excellent machi.. |