Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.4 µm/m-°C @Temperature 250 °C |
6.91 µin/in-°F @Temperature 482 °F |
|
Mykroy/Mycalex MM 501 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwide.. |