Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.4 µm/m-°C @Temperature 26.7 - 427 °C |
6.90 µin/in-°F @Temperature 80.0 - 800 °F |
|
International Mold Steel Premium H13 Hot Work Die and Mold Steel Description: International Mold Steel's Premium H-13 is a chromium-based, hot work die and plastic mold steel designed for increased production rates and longer tool life. It meets the restricti.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 21.1 - 204 °C |
6.90 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel Description: Thermodur® 2367 Superclean is an electro slag remelted (ESR) hot work die steel developed for applications where high temperature properties (tensile strength & thermal conductivity).. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 21.1 - 204 °C |
6.90 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Thermodur® E38K Hot Work Die Steel Description: Thermodur® E38K is an electro slag remelted (ESR) modified H-11 die steel, developed for hot working applications where maximum mechanical strength (toughness) properties are require.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 399 °C |
6.90 µin/in-°F @Temperature 68.0 - 750 °F |
|
EDRO #7 Shock Resistant S7 Tool Steel EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 538 °C |
6.90 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Crucible Steel CRUCIBLE A9 Tool Steel Crucible A9 is an air-hardening tool steel combining some of characteristics of the 5% chromium hot-work grades (such as H13) with the high attainable hardness and compressive yield strength of the .. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 21.1 - 204 °C |
6.90 µin/in-°F @Temperature 70.0 - 400 °F |
|
Crucible Steel CSM® 21 17Cr-4Ni Precipitation Hardening Stainless Steel CSM 21 is a precipitation hardening stainless mold steel, providing outstanding corrosion resistance and toughness, good polishability, and moderate wear resistance, combined with simple heat treatm.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 20.0 - 204 °C |
6.90 µin/in-°F @Temperature 68.0 - 400 °F |
|
Crucible Steel CSM® 6 Tool Steel, AISI A6 CSM 6 is an air hardening tool steel offering moderate wear resistance and toughness. It may be hardened from a low hardening temperature for easy heat treatment.Information provided by Crucible Ind.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 21.1 - 427 °C |
6.90 µin/in-°F @Temperature 70.0 - 800 °F |
|
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11 Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly su.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 399 °C |
6.90 µin/in-°F @Temperature 750 °F |
hardened to 57 HRC |
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel Chromium-molybdenum alloyed steelA versatile S7 grade recommended for applications demanding a high degree of toughness and moderate wear resistance. Successfully used for heavy-duty punching and sh.. |
|||
CTE, linear | 12.4 µm/m-°C @Temperature 21.1 - 204 °C |
6.90 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel Description: Thermodur® 2343 is a single melt Extra Fine Structure (EFS) hot work die steel and Supplied in the annealed conditionCharacteristics: Good toughness; Moderate high-temperature strength.. |