CTE, linear 12.25 µm/m-°C

@Temperature 24.0 - 316 °C
6.806 µin/in-°F

@Temperature 75.2 - 601 °F
Latrobe Lesco 53 VIM-VAR Premium Carburizing Steel
LESCO 53 VIM-VAR is a premium quality alloy carburizing gear steel designed to resist softening at elevated service temperatures. It is double vacuum processed by vacuum induction melting followed ..