Thermal Properties Metric English Comments
CTE, linear 12.15 µm/m-°C

@Temperature 21.0 - 93.0 °C
6.750 µin/in-°F

@Temperature 69.8 - 199 °F
Mean; Annealed and Aged
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed
Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Heat capacity, melting range, moduli, and Poisson's ratio re..
CTE, linear 12.15 µm/m-°C

@Temperature 21.0 - 93.0 °C
6.750 µin/in-°F

@Temperature 69.8 - 199 °F
Mean
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed + Aged
Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Typical aging - 1750°F (954°C)/1 h/AC plus 1325°F (..