Thermal Properties Metric English Comments
CTE, linear 11.03 µm/m-°C

@Temperature 21.0 - 149 °C
6.128 µin/in-°F

@Temperature 69.8 - 300 °F
Latrobe Lescalloy® BG42 VIM-VAR High Performance Bearing Steel
LESCALLOY BG42 VIM-VAR steel is a martensitic, stainless high speed steel that combines the tempering, hot hardness and hardness retention characteristics of M50 high speed steel with the corrosion ..