Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 55.1 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E831 |
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet) KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. .. |
|||
CTE, linear | 55.1 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E831 |
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet) KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re.. |
|||
CTE, linear | 55.1 µm/m-°C @Temperature 121 °C |
30.6 µin/in-°F @Temperature 250 °F |
ASTM D696 |
Dow SPECTRIM™ HH 390 Reaction Moldable Polymer Information provided by Dow |
|||
CTE, linear | 55.1 µm/m-°C @Temperature 50.0 - 185 °C |
30.6 µin/in-°F @Temperature 122 - 365 °F |
Z-Axis Alpha 1; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW.. |