Thermal Properties Metric English Comments
CTE, linear 97.0 µm/m-°C

@Temperature 50.0 - 70.0 °C
53.9 µin/in-°F

@Temperature 122 - 158 °F
MD; ASTM D696
DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film
Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o..
CTE, linear 97.0 µm/m-°C

@Temperature 25.0 - 50.0 °C
53.9 µin/in-°F

@Temperature 77.0 - 122 °F
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic
High clarity plastic for a multitude of applicationsFeaturesClear and transparentRigid and toughGreat for headlamps, bottles and transparent assembliesExcellent humidity/moisture resistanceAll infor..
CTE, linear 97.0 µm/m-°C

@Temperature -40.0 °C
53.9 µin/in-°F

@Temperature -40.0 °F
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
CTE, linear 97.0 µm/m-°C

@Temperature -40.0 °C
53.9 µin/in-°F

@Temperature -40.0 °F
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..