Thermal Properties Metric English Comments
CTE, linear 10.20 µm/m-°C

@Temperature 25.0 °C
5.667 µin/in-°F

@Temperature 77.0 °F
Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite