Polymer Property : CTE, linear = 5.34 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 9.61 µm/m-°C

@Temperature 37.8 - 260 °C
5.34 µin/in-°F

@Temperature 100 - 500 °F
Crucible Steel REX® M7N High Speed Steel, AISI M7
REX M7 is molybdenum type high speed steel designed with higher carbon and vanadium to provide higher hardness after heat treatment and improved wear resistance compared to M1 steel.Information prov..