CTE, linear 9.32 µm/m-°C

@Temperature 24.0 - 204 °C
5.18 µin/in-°F

@Temperature 75.2 - 399 °F
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core
Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the ..