CTE, linear | 8.50 - 9.20 µm/m-°C @Temperature 30.0 - 350 °C |
4.72 - 5.11 µin/in-°F @Temperature 86.0 - 662 °F |
|
ATI Allegheny Ludlum AL 4750™ Electrical Alloy, UNS K94800 or UNS K95000 The alloy produces good magnetic properties, wide latitude to control hysteresis loop shape via recrystallization modes. Applications for this grade range from electromechanical relay cores, to ver.. |