Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 87.0 µm/m-°C @Temperature 100 - 200 °C |
48.3 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
3M Dyneon™ 1750 PTFE Powder
(discontinued **) Type II PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r.. |
|||
CTE, linear | 87.0 µm/m-°C @Temperature 100 - 200 °C |
48.3 µin/in-°F @Temperature 212 - 392 °F |
ASTM D1530 |
3M Dyneon™ 1620 PTFE Powder
(discontinued **) Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
CTE, linear | 87.0 µm/m-°C @Temperature 100 - 200 °C |
48.3 µin/in-°F @Temperature 212 - 392 °F |
ASTM E1530 |
3M Dyneon™ 1641 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
CTE, linear | 87.0 µm/m-°C @Temperature 100 - 200 °C |
48.3 µin/in-°F @Temperature 212 - 392 °F |
ASTM E1530 |
3M Dyneon™ 1645 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
CTE, linear | 87.0 µm/m-°C @Temperature 0.000 - 20.0 °C |
48.3 µin/in-°F @Temperature 32.0 - 68.0 °F |
T<Tg; ASTM E831-93 |
3D Systems Accura® 40 Plastic for SLA® Systems 40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components a.. |