Thermal Properties Metric English Comments
CTE, linear 82.5 µm/m-°C

@Temperature 200 - 300 °C
45.8 µin/in-°F

@Temperature 392 - 572 °F
ASTM E-233
UBE UPIMOL® R Polyimide Shape
Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub..