Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.89 µm/m-°C @Temperature 20.0 - 100 °C |
4.94 µin/in-°F @Temperature 68.0 - 212 °F |
|
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel Description: DH2F is one of the best machining pre-hardened H13-type steels available.Unique Characteristics: 38-42 HRc hardness.Through hardened for exceptional dimensional stability.Cuts mold maki.. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 250 °C |
4.94 µin/in-°F @Temperature 482 °F |
upon cooling |
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 20.0 - 300 °C |
4.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott BG38 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 20.0 - 300 °C |
4.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott F5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 20.0 - 300 °C |
4.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott P-SK57 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 20.0 - 300 °C |
4.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott SF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 20.0 - 300 °C |
4.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott UG1 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature >=316 °C |
4.94 µin/in-°F @Temperature >=601 °F |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 538°C High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature >=316 °C |
4.94 µin/in-°F @Temperature >=601 °F |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 593°C High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature >=316 °C |
4.94 µin/in-°F @Temperature >=601 °F |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Annealed Strip/Sheet High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature >=316 °C |
4.94 µin/in-°F @Temperature >=601 °F |
|
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Overaged High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 25.0 - 700 °C |
4.94 µin/in-°F @Temperature 77.0 - 1290 °F |
|
CeramTec 645 Steatite (MgO-SiO2) Te value is 810°C. Hasselman Thermal Shock value is 600 K.Data provided by CeramTec North America. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.94 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG23 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |