Polymer Property : CTE, linear = 4.93 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 8.88 µm/m-°C

@Temperature 300 °C
4.93 µin/in-°F

@Temperature 572 °F
Plansee CFY Chromium-Iron-Yttrium
The most typical use for CFY is as interconnects in fuel cells.Characteristics: Coefficient of expansion - designed for compatibility with that of the electrolyte in fuel cells Corrosion resistance..