Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.86 µm/m-°C @Temperature 149 °C |
2.70 µin/in-°F @Temperature 300 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 705 Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other .. |
|||
CTE, linear | 4.86 µm/m-°C @Temperature -30.0 - 30.0 °C |
2.70 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D-696 |
Axiall 7055 Rigid PVC, Extrusion, White Georgia Gulf 7055 White is a special purpose rigid PVC extrusion compound designed for window and door applications. The compound exhibits the following characteristics: WeatherabilityChemical Res.. |