Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.00 - 4.70 µm/m-°C @Temperature 30.0 - 300 °C |
2.22 - 2.61 µin/in-°F @Temperature 86.0 - 572 °F |
|
ATI Allegheny Ludlum AL 42™ Electrical Alloy, UNS K94100 AL 42 alloy is used extensively in the manufacture of sealed beam automobile head lamps, in grommet and pin type glass-metal seals, and in integrated circuit lead frames. It is also the core metal .. |